Sustainable Stabilization of Soft Clay Using a Hybrid Cement–alkali Activated Waste-glass Binder: Strength, Compressibility and Microstructural Performance
Аннотация
Soft clay deposits typically exhibit low undrained shear strength and high compressibility, often requiring stabilization before construction. This study investigates a hybrid binder system combining 5% ordinary Portland cement with a waste-glass-based geopolymer produced from recycled glass powder and sodium silicate activator. Glass powder contents of 5–20% and sodium silicate contents of 0.5–2% were evaluated in soft-clay specimens treated with the hybrid cement–alkali-activated waste-glass binder using unconfined compressive strength, one-dimensional consolidation, and selected scanning electron microscopy tests. Cement-only treatment increased the 28-day unconfined compressive strength to 323, 410, and 515 kPa for 5%, 10%, and 15% cement, respectively. Adding recycled glass powder and sodium silicate markedly improved strength. The optimum mixture, containing 5% cement, 20% glass powder, and 1% sodium silicate, reached a 28-day strength of 1172 kPa, corresponding to approximately 3.6, 2.9, and 2.3 times the strengths achieved with 5%, 10%, and 15% cement alone, respectively. The strength gain is attributed to the combined effects of cement hydration and reactions involving alkali-activated waste glass, which produce binding products that strengthen particle contacts and fill pore spaces. The optimum mixture reduced the compression index (Cc) from 0.4475 for the untreated soil to 0.0719 and the swell index (Cs) from 0.0526 to 0.0015, demonstrating substantial improvements in resistance to compression and swelling. For all glass-powder contents, 1% sodium silicate produced the most favorable strength and consolidation response, whereas higher activator dosages reduced performance. Finally, SEM observations showed a denser, more cemented soil fabric, with gel-like products coating and bonding clay particles. Graphical abstract