Effect of Polymeric Coatings on the Deformation Behaviour of Low-Nickel Austenitic Stainless Steel in Air and Hydrogen Environments
Аннотация
The increasing use of hydrogen as a clean energy carrier has created a need for cost-effective structural materials with reliable resistance to hydrogen-assisted degradation. A key challenge is that high-nickel austenitic 316 stainless steels (SS), although more resistant to hydrogen embrittlement (HE), are significantly more expensive than low-nickel grades. Therefore, low-nickel austenitic stainless steels offer a potential cost advantage. However, their susceptibility to HE remains a challenge. Polymeric barrier coatings are being explored as a possible strategy to mitigate HE and improve material performance, but their influence on the hydrogen-assisted deformation behaviour of 316 SS remains insufficiently understood. This study investigates the influence of polytetrafluoroethylene (PTFE) and polyurethane (PU) coatings on the deformation and fracture behaviour of 316 SS in air and hydrogen environments. Slow strain rate tests were conducted at a strain rate of 2 × 10⁻⁴ mm/s under 10 MPa hydrogen at 20 ± 1 °C. In air, uncoated 316 SS exhibited high ductility, with 46.0% elongation and 83.3% reduction in area, whereas PTFE and PU coated specimens showed reduced ductility. Hydrogen exposure further decreased the elongation and reduction in area of coated specimens, indicating greater susceptibility to HE. The ultimate tensile strength decreased for uncoated 316 SS but increased for coated specimens under hydrogen. Oxygen-nitrogen-hydrogen analysis indicated greater hydrogen retention in coated specimens. Fractographic examination revealed hydrogen-assisted cracking and premature failure. Overall, under the investigated conditions, PTFE and PU coatings did not mitigate HE. Instead, the coated specimens exhibited greater susceptibility to HE than uncoated 316 SS.