Fretting Wear and Peel Load of TiN and TiZrN Coatings

Science China Physics, Mechanics & Astronomy · Springer Nature · 2026-04-01 · DOI: 10.3103/S1068366626700327

Аннотация

Abstract The influence of the structure, physicomechanical properties, and annealing of TiN and TiZrN coatings on their resistance to fretting wear and spalling was investigated. It was established that low-temperature annealing of TiN coatings in air leads to an increase in their spalling load and wear resistance under fretting conditions. It was concluded that the formation of a thin film of lower titanium oxides on the coating surface during low-temperature annealing, which possess solid lubricant properties, contributes to the increase in spalling load and fretting wear resistance. It was shown that the spalling load for TiN coatings increases with an increase in substrate hardness. It was concluded that the accumulation of plastic shifts in a soft substrate during scratch testing leads to the emergence of tensile stresses in the high-strength surface layer and a decrease in its spalling load. It was established that low-temperature annealing at 350–400°C of a TiN coating increases its wear resistance under dry friction conditions by ≈10% compared to the coating’s initial state. High-temperature annealing at 450–550°C, conversely, leads to increased wear (up to ≈ 17%). It was concluded that the intensification of fretting wear after high temperature annealing at 550°C is caused by the softening of the coating, a decrease in its spalling load, and the ingress of hard and brittle TiO 2 oxide particles into the friction zone. It was established that the wear resistance of a magnetron-sputtered TiZrN coating exceeds the resistance to fretting wear of a vacuum-arc deposited TiN coating, which is associated with the higher level of strength properties of the TiZrN coating. It was shown that during the friction of TiN and TiZrN coatings in a 5% aqueous NaCl solution and in water, the intensity of fretting wear decreases by ≈10% compared to friction without a lubricant, which is due to the presence of a water layer between the friction surfaces, preventing their adhesive interaction. At the same time, the high corrosion resistance of the TiN coating prevents the development of fretting-corrosion during tests.

Читать у издателя →

Похожие статьи