Experimental investigations on mechanical properties and microstructure during joining Inconel 800 and SS310 by friction welding

Archives of Orthopaedic and Trauma Surgery · Springer Nature · 2026-11-18 · DOI: 10.1007/s43538-026-00969-7

Аннотация

Friction welding has demonstrated significant potential for joining dissimilar materials; however, limited research exists on the difficulties involved in welding various material combinations. By focusing on Inconel 800 and SS310, the objective is to assess the effects of important welding parameters on microstructure, microhardness, and joint strength. Inconel 800 and SS310 specimens were subjected to experimental friction welding while varying crucial process parameters, including friction pressure and rotation speed. Tensile testing was conducted to assess the strength of the welded joints. The heat-affected zone (HAZ) and thermomechanically affected zone (TMAZ) were identified by microstructural analysis, followed by microhardness studies to assess their influence on hardness distribution. The results demonstrated that the welding conditions significantly affected the mechanical and microstructural properties of the joints. The highest tensile strength of 636.618 MPa was achieved at a friction pressure of 5.5 MPa and a rotational speed of 1500 rpm; the lowest tensile strength of 108.989 MPa was obtained at a friction pressure of 5.5 MPa and a rotational speed of 870 rpm. Higher-strength joints’ microstructural analysis revealed discrete zones with fine, equiaxed grains near the weld contact, including the HAZ and TMAZ. Variations in rotational speed and friction pressure have a substantial effect on the microstructure, causing phase shifts and the development of carbide precipitates that ultimately change the mechanical properties of the weld region. Due to the presence of fine grains and the formation of a carbide layer, the micro-hardness at the weld interface is higher than in the TMAZ and HAZ. The study demonstrates that selecting optimal friction-welding conditions can enhance joint strength and durability, thereby expanding the process’s capabilities in sectors that require high-performance material combinations.

Читать у издателя →

Похожие статьи