Optimizing cerium in bismuth oxide nanophotocatalyst for efficient photocatalytic activity and hydrogen evolution
Аннотация
A heterojunction of bismuth–cerium oxide (Bi–Ce oxide) with the appropriate band edge location in relation to the redox potential for dissociating water to produce hydrogen is anticipated to exhibit excellent photocatalytic activity across a wide range of solar irradiation. In this study, a series of Bi–Ce oxide hetero-nanocomposite photocatalyst with different cerium content (0–10%) was synthesized via the hydrothermal method. Initially, the cerium content in Bi–Ce oxide was optimized for superior visible light photocatalytic activity through degradation kinetics of probe dyes. The effect of Ce content on structural morphology and optical characteristics of the Bi–Ce oxide composite was analysed for correlating them with the degradation kinetics. The results were conclusively explained and corroborated using the characterization results of X-ray diffractometer (XRD), UV–Vis DRS spectrophotometer, scanning electron microscopy (SEM), thermo-gravimetric and differential thermal analyser (TGA-DTA), X-ray photoelectron spectroscopy (XPS), transmission electron microscopy (TEM), photoluminescence (PL) spectrophotometer, and time-resolved PL (TRPL) in addition to gas chromatograph (GC). The degradation kinetics of rhodamine-B (RhB) and methylene blue (MB) were used to measure the photocatalytic activity of the photocatalysts. It demonstrates that under visible irradiation, the sample with the maximum photoactivity (~ 1.65 to 1.81 times the pure Bi-oxide) has a 2% Ce content (bandgap ~ 2.62 eV). The relative enhancement in the hydrogen evolution kinetics with the optimized sample was 3.6-fold compared to the pristine Bi-oxide under solar irradiation. The primary reason for the improved activity of the sample was the optimized Bi–Ce ratio with resultant oxygen vacancies/defects, suitable hexagonal nanosheet morphology, lower binding energy, improved carrier lifetime (1.26 times) and the apposite band edge location.