The Feasibility of Atomic Layer Deposition of Aluminum Oxide on TATB
Abstract
ABSTRACT Plastic‐bonded explosive (PBX) formulations are physical mixtures of polymers with explosive solids, and their mechanical strength is heavily dependent on the adhesion between polymer and explosive. The surface chemistry of the explosive can limit the strength of this bond. This paper explores the capability of atomic layer deposition (ALD) to successfully coat a representative explosive powder (triaminotrinitrobenzene, TATB) to generate a new surface functionality without degrading the explosive crystal. ALD is a thin film deposition technique designed to coat high aspect ratio materials conformally with sub‐nm level precision by utilizing alternating exposures of gaseous species to form monolayer reaction sequences on the substrate of interest's surface. X‐ray photoelectron spectroscopy of a batch of TATB crystals coated with 20 deposition cycles of aluminum oxide reveal the presence of the Al 2s and 2p peaks, as well as oxygen peaks, consistent with successful aluminum oxide deposition. Transmission electron imaging after focused ion beam lift‐out reveals the presence of approximately an 80 nm coating after 200 ALD cycles, corresponding to a deposition rate of about 4 Å/cycle. Finally, small‐scale safety testing for thermal, impact, spark, friction, and chemical aging were performed on TATB processed with 20 cycles of aluminum oxide ALD. Coated TATB was demonstrated to be insensitive with some slight increase thermal aging mediated degradation. In summary, this shows that ALD is likely usable on explosives without catastrophic chemical effects, and the effects of the surface changes will be useful for PBX formulation processes.