Emilio Mello, Laura Meda, Mario Salvalaggio. Surface analysis and considerations on the Marcus Aurelius equestrian-statue gilding. // Archaeological and Anthropological Sciences. – 2026. – DOI: 10.1007/s12520-025-02385-2. – URL: https://doi.org/10.1007/s12520-025-02385-2
Emilio Mello, Laura Meda, & Mario Salvalaggio (2026). Surface analysis and considerations on the Marcus Aurelius equestrian-statue gilding. Archaeological and Anthropological Sciences. https://doi.org/10.1007/s12520-025-02385-2
Emilio Mello, et al. “Surface analysis and considerations on the Marcus Aurelius equestrian-statue gilding.” Archaeological and Anthropological Sciences, 2026. doi:10.1007/s12520-025-02385-2.
@article{Mello2026,
title = {Surface analysis and considerations on the Marcus Aurelius equestrian-statue gilding},
author = {Mello, Emilio and Meda, Laura and Salvalaggio, Mario},
journal = {Archaeological and Anthropological Sciences},
year = {2026},
doi = {10.1007/s12520-025-02385-2},
url = {https://doi.org/10.1007/s12520-025-02385-2}
}