Spark Plasma Sintering of Inconel 718 Superalloy Powder Synthesized by Mechanical Alloying of Elemental Powders
Polasani Ajay, Himanshu Pal, Vikram V. Dabhade, S. V. S. Narayana Murty, Sushant Manwatkar
Springer Nature ·
2026-09-03
· DOI 10.1007/s11665-026-14960-2
The publisher did not provide an abstract — full text is available via the link below.
Polasani Ajay, Himanshu Pal, Vikram V. Dabhade, S. V. S. Narayana Murty, Sushant Manwatkar. Spark Plasma Sintering of Inconel 718 Superalloy Powder Synthesized by Mechanical Alloying of Elemental Powders. // Journal of Materials Engineering and Performance. – 2026. – DOI: 10.1007/s11665-026-14960-2. – URL: https://doi.org/10.1007/s11665-026-14960-2
Polasani Ajay, Himanshu Pal, Vikram V. Dabhade, S. V. S. Narayana Murty, & Sushant Manwatkar (2026). Spark Plasma Sintering of Inconel 718 Superalloy Powder Synthesized by Mechanical Alloying of Elemental Powders. Journal of Materials Engineering and Performance. https://doi.org/10.1007/s11665-026-14960-2
Polasani Ajay, et al. “Spark Plasma Sintering of Inconel 718 Superalloy Powder Synthesized by Mechanical Alloying of Elemental Powders.” Journal of Materials Engineering and Performance, 2026. doi:10.1007/s11665-026-14960-2.
@article{Ajay2026,
title = {Spark Plasma Sintering of Inconel 718 Superalloy Powder Synthesized by Mechanical Alloying of Elemental Powders},
author = {Ajay, Polasani and Pal, Himanshu and Dabhade, Vikram V. and Murty, S. V. S. Narayana and Manwatkar, Sushant},
journal = {Journal of Materials Engineering and Performance},
year = {2026},
doi = {10.1007/s11665-026-14960-2},
url = {https://doi.org/10.1007/s11665-026-14960-2}
}