Julien Prouteau, Florence Hamon, Patrick Villechaise, Anchal Goyal, Jonathan Cormier. Mechanical Properties of the Polycrystalline γ/γ′ Nickel-Based Superalloy René 65 After Long-Term Aging. // Metallurgical and Materials Transactions A. – 2026. – DOI: 10.1007/s11661-026-08118-x. – URL: https://doi.org/10.1007/s11661-026-08118-x
Julien Prouteau, Florence Hamon, Patrick Villechaise, Anchal Goyal, & Jonathan Cormier (2026). Mechanical Properties of the Polycrystalline γ/γ′ Nickel-Based Superalloy René 65 After Long-Term Aging. Metallurgical and Materials Transactions A. https://doi.org/10.1007/s11661-026-08118-x
Julien Prouteau, et al. “Mechanical Properties of the Polycrystalline γ/γ′ Nickel-Based Superalloy René 65 After Long-Term Aging.” Metallurgical and Materials Transactions A, 2026. doi:10.1007/s11661-026-08118-x.
@article{Prouteau2026,
title = {Mechanical Properties of the Polycrystalline γ/γ′ Nickel-Based Superalloy René 65 After Long-Term Aging},
author = {Prouteau, Julien and Hamon, Florence and Villechaise, Patrick and Goyal, Anchal and Cormier, Jonathan},
journal = {Metallurgical and Materials Transactions A},
year = {2026},
doi = {10.1007/s11661-026-08118-x},
url = {https://doi.org/10.1007/s11661-026-08118-x}
}