Densification Behavior and Microstructures of β-Si_3N_4/O'-SiAlON Composites Prepared by Spark Plasma Sintering

Huang, Yi-Chi, Lee, Alex C. H., Lu, Horng-Hwa, Huang, Jow-Lay
Springer Nature · 2026-01-01 · DOI 10.1007/s11106-026-00547-y

Abstract

Nanoscale Si_3N_4 powder facilitates densification at lower sintering temperatures, allowing sintered bodies to more readily approach theoretical density and achieve nanoscale microstructures. In this study, amorphous nanoscale Si_3N_4 powder was used as the starting material and consolidated via spark plasma sintering (SPS) at a heating rate of 100°C/min to investigate the effects of rapid sintering on phase ratio, microstructure, and mechanical properties. A fully densified 62% Si_3N_4/38% O'-SiAlON composite ceramic can be achieved in 16 min. These characteristics were also compared with those of samples prepared by hot pressing at a heating rate of 10°C/min. At a sintering temperature of 1800°C, the β-Si_3N_4 phase dominated in both methods. SPS promoted the formation of elongated rod-like grains while preserving a submicron matrix, thereby increasing the aspect ratio. Consequently, the SPS method not only improved the toughness of the Si_3N_4-based composites but also maintained high hardness due to the strong matrix.

Read at publisher →