Journal of Sustainable Metallurgy Металлы и сплавы
Chloride Salt-Based Brine Leaching of Precious Metals and Other Valuable Metals from Secondary Resources for Reduced Hydrochloric Acid Consumption
Аннотация
Abstract Copper-leaching residues generated from secondary resources, such as waste printed circuit boards, contain precious metals and other elements such as Sb and Sn. Conventional HCl-based leaching requires high acid input, leading to elevated HCl consumption and insufficient selectivity. This study investigates chloride-salt-assisted “brine leaching” as an alternative for reducing HCl consumption while enhancing the recovery of Au, Pd, Pt, Sn, and Sb. Leaching tests were conducted using NaCl, CaCl 2 , and KCl under controlled potential and pH conditions. The results showed that when utilizing HCl concentrations above 2 mol/L, leaching rates exceeding 90% were achieved for Au, Pd, Pt, and Sn. However, at concentrations below 2 mol/L, the dissolution of Au, Pd, Pt, and Sn was suppressed, and only a small fraction of Sb was leached. For NaCl, the leaching rates of Au, Pd, Pt, and Sn exceeded 90% at acid concentrations below 2 mol/L, with Sb dissolution limited to less than 1%. Equilibrium analysis and speciation modeling indicated that Sn dissolved predominantly as Sn(IV) chloro-complexes, whereas Sb formed sparingly soluble Sb(V) complex oxide (Na,H) 14 Sb 14 O 21 (OH) 42 , confirmed by X-ray diffraction observations. For the total Cl − ions in the 3–5 mol/L range, the consumption of HCl was very low or almost nonexistent, demonstrating that chloride salts can provide the necessary Cl − for the formation of stable chloro complexes while minimizing HCl consumption. These findings demonstrate the potential of brine leaching as a new environmentally friendly processing method to effectively leach precious metals while reducing the consumption of HCl using chloride salts.