npj Materials Degradation Materials Chemistry

PVD Ce-coating to mitigate intergranular oxidation of additively manufactured Ni-base alloy IN625

A. Chyrkin, A. Fazi, M. Sattari, M. Thuvander, K. Stiller, M. Halvarsson, E. Wessel, D. Naumenko, J. Froitzheim
Springer Nature · 2025-09-29 · DOI 10.1038/s41529-025-00677-5

Abstract

Abstract Additively manufactured Ni-base alloy IN625 suffered from intergranular oxidation (IGO) during air exposure at 900 °C. IGO is triggered by oxide buckling over the alloy’s grain boundaries (GBs), followed by oxidation of the open intergranular voids. Application of a 10 nm thick PVD coating of Ce induced a slower inward growth of the Cr 2 O 3 scale, better oxide adherence and as a result strongly suppressed IGO. The main beneficial effect provided by Ce is improved oxide adherence preventing oxide buckling and oxidation of intergranular voids.

Read at publisher →