Polymer Composites Керамика и композиты

Failure Mode Transition Mechanism and Strength Prediction for Multi‐Bolted Double‐Shear GLARE Joints

Shiming Zu, Yuanqing Deng, Pengcheng Wang, Jiyuan Zhang, Mengyang Xie, Haijiao Wang, Xueyou Tan, Zhengong Zhou
Wiley · 2026-11-19 · DOI 10.1002/pc.71862

Аннотация

ABSTRACT Multi‐bolt joints are critical structural connections in primary aeronautical load‐bearing components, whose efficiency directly governs aircraft structural safety and weight reduction. Conventional strength prediction methods often misjudge failure modes owing to their inability to capture dynamic coupling between internal damage evolution and load redistribution across fastener rows. This work investigates the mechanical performance and joint efficiency of single‐bolt up to four‐bolt double‐shear GLARE 5‐3/2‐0.4 laminate joints through quasi‐static tensile tests and a three‐dimensional progressive damage finite element (FE) model. Experimental and numerical results identify a prominent failure‐mechanism transition with increasing bolt count: single‐bolt and two‐bolt joints experience progressive bearing failure with good ductility and energy absorption, while three‐bolt and four‐bolt joints suffer catastrophic net‐tension failure initiated by longitudinal fiber rupture near the outermost bolt hole. Simulations attribute this phenomenon to severe load maldistribution that triggers premature stress concentration and local stiffness degradation at this critical hole. An average load ratio (ALR) method is proposed for stable damage evolution stages. It corrects two‐bolt failure‐mode misjudgment and maintains multi‐bolt errors within 15%, though not consistently superior. Overall, this work provides a reliable prediction framework and practical design guidance, though currently limited to the investigated GLARE laminate and geometry.

Читать у издателя →