Y.Y. Chang, J.T. Zhang, X.J. Jiang, Y.F. Jia. Effect of compression deformation on the pitting corrosion behavior of an as-forged Ti-6Al-4V-30Zr alloy in Cl--containing environments. // Surfaces and Interfaces. – 2026. – DOI: 10.1016/j.surfin.2025.108349. – URL: https://doi.org/10.1016/j.surfin.2025.108349
Y.Y. Chang, J.T. Zhang, X.J. Jiang, & Y.F. Jia (2026). Effect of compression deformation on the pitting corrosion behavior of an as-forged Ti-6Al-4V-30Zr alloy in Cl--containing environments. Surfaces and Interfaces. https://doi.org/10.1016/j.surfin.2025.108349
Y.Y. Chang, et al. “Effect of compression deformation on the pitting corrosion behavior of an as-forged Ti-6Al-4V-30Zr alloy in Cl--containing environments.” Surfaces and Interfaces, 2026. doi:10.1016/j.surfin.2025.108349.
@article{Chang2026,
title = {Effect of compression deformation on the pitting corrosion behavior of an as-forged Ti-6Al-4V-30Zr alloy in Cl--containing environments},
author = {Chang, Y.Y. and Zhang, J.T. and Jiang, X.J. and Jia, Y.F.},
journal = {Surfaces and Interfaces},
year = {2026},
doi = {10.1016/j.surfin.2025.108349},
url = {https://doi.org/10.1016/j.surfin.2025.108349}
}