Investigation of wear behavior by the addition of hard powder to Stellite powder in hardfacing of steel by gas tungsten arc welding

Nature Reviews Methods Primers · Springer Nature · 2026-09-21 · DOI: 10.1007/s00161-026-01526-9

Аннотация

Hardfacing by gas tungsten arc welding (GTAW) is widely used to produce hard, wear-resistant surfaces on components such as valves and drills. Here, cobalt-based Stellite 1 was reinforced with silicon carbide (SiC, 10–50 wt.%, mesh 15–140) and deposited on ST12 carbon steel by pulsed GTAW; the pulsed current, SiC particle size, and SiC content were optimized in sequence to maximize coating hardness. The optimum coating (30 wt.% SiC, 50–80 mesh, 110–180 A pulsed current) reached a macro-hardness of ~1293 HV10—roughly three times that of the carbide-free Stellite 1 coating (~ 400 HV10) and six times that of the uncoated substrate (~ 200 HV10). Microstructural analysis (optical and scanning electron microscopy, EDS) showed that this hardness increase is governed primarily by the degree of dendritic development of the coating rather than by SiC content alone, with SiC additions above 30 wt.% promoting spheroidization of interdendritic phases and a marked hardness decrease. X-ray diffraction identified Fe8Si2C, Cr7C3 and Co6W6C as the principal strengthening phases, together with Cr2O3·FeO and CoFe arising from substrate dilution and surface oxidation. Under dry pin-on-disk wear testing (10 N and 15 N against an AISI 52100 counterface), the optimum coating lost less mass than the steel pin and showed a friction coefficient of 0.3–0.4, roughly double that of the carbide-free coating, with adhesive wear accompanied by oxide formation as the dominant mechanism. These results show that, when correctly optimized, SiC reinforcement of Stellite 1 hardfacing coatings provides a substantial and reproducible improvement in surface hardness and wear resistance over the unreinforced alloy.

Читать у издателя →

Похожие статьи