Modifying Caking Index of Shenfeng Long-Flame Coal: A Low-Temperature Thermal Treatment

Journal of Umm Al-Qura University for Applied Sciences · Springer Nature · 2026-07-01 · DOI: 10.3103/S1068364X26600612

Аннотация

Abstract A low-temperature thermal (LT) treatment was used to enhance the caking index ( G ) of Shenfeng long-flame coal (SF). To identify the underlying factors governing the caking behavior of SF, SF and its pyrolysis residues obtained at various temperatures were characterized by Fourier transform infrared spectroscopy, solid-state 13 C nuclear magnetic resonance (NMR) spectroscopy, and Raman spectroscopy. The results demonstrated that LT treatment significantly elevated the G value of SF, with a clear upward trend as the treatment temperature increased, eventually reaching a plateau in the temperature range of 450–500°C. This improvement is attributed to two synergistic effects. First, the thermal process promotes the removal of oxygen-containing functional groups and aliphatic side chains, while simultaneously facilitating the condensation polymerization of aromatic rings, which collectively convert the originally weakly caking coal into a relatively strongly caking material. Second, the Raman spectral evolution and the solid-state 13 C NMR results revealed a deepened graphitization degree after LT treatment, indicating that the structural order of the carbon skeleton was enhanced. These complementary modifications jointly account for the increase in the G value.

Читать у издателя →

Похожие статьи