Dewaxing of Pyrolysis Oil over a Bifunctional Ni/(HZSM-5 + Al 2 O 3 ) Catalyst as a Method for Hydroprocessing Plastic Waste

Chemistry and Biodiversity · Wiley · 2026-10-01 · DOI: 10.1134/S0965544126601390

Аннотация

Abstract A composite 7.5% Ni/(50% HZSM-5 + 50% γ,η-Al 2 O 3 ) catalyst was synthesized for hydroisodewaxing of the kerosene–diesel fraction of pyrolysis oil obtained from polyethylene and polypropylene waste. Medium-pore ZSM-5 zeolite (Si/Al = 40), prepared by the hydrothermal method, was used as the acid component. The catalyst was tested in hydroprocessing of the pyrolysis oil fraction at T = 320, 340, and 360°C, P (H 2 ) = 40 bar, LHSV = 1 h –1 , and H 2 /feed = 1000 L (20°C, 1 atm)/L (20°C). With Ni as the active component, alkenes and dienes were almost completely hydrogenated to a residual content of no more than 1–2%, whereas dewaxing of the feedstock proceeded on the acid sites of ZSM-5 zeolite through isomerization and selective cracking of n -alkanes owing to the molecular-sieve selectivity toward unbranched molecules. With increasing temperature, the iso -/ n -alkane ratio rose from 0.3 in the feedstock to 0.7 at 320°C and to 1.5–1.6 at 340–360°C, while the n -paraffin content in the kerosene–diesel fraction decreased to 1–2% in the C 9+ range and high-boiling C 15 –C 16 n -paraffins were completely removed. More extensive dewaxing with increasing temperature was accompanied by lower selectivity to iso -alkanes because of enhanced cracking of n -alkanes with gas formation, accumulation of cyclic and aromatic compounds, and catalyst coking. The optimal balance between the extent of hydroisodewaxing and the yield of middle distillates was achieved at 320°C, which provides a cloud point of −10°C; this demonstrates the potential of the developed catalyst for hydroprocessing pyrolysis oil into motor-fuel components with improved low-temperature properties.

Читать у издателя →

Похожие статьи