Renfeng Jiang, Qing Huang, Weiqiang Su, Haibin Liu, Xiaomao Dong, Mengwu Wu. Casting Defect Detection and Segmentation in X-ray Images Based on SAHI and YOLO11-seg Algorithms. // International Journal of Metalcasting. – 2026. – DOI: 10.1007/s40962-026-02058-3. – URL: https://doi.org/10.1007/s40962-026-02058-3
Renfeng Jiang, Qing Huang, Weiqiang Su, Haibin Liu, Xiaomao Dong, & Mengwu Wu (2026). Casting Defect Detection and Segmentation in X-ray Images Based on SAHI and YOLO11-seg Algorithms. International Journal of Metalcasting. https://doi.org/10.1007/s40962-026-02058-3
Renfeng Jiang, et al. “Casting Defect Detection and Segmentation in X-ray Images Based on SAHI and YOLO11-seg Algorithms.” International Journal of Metalcasting, 2026. doi:10.1007/s40962-026-02058-3.
@article{Jiang2026,
title = {Casting Defect Detection and Segmentation in X-ray Images Based on SAHI and YOLO11-seg Algorithms},
author = {Jiang, Renfeng and Huang, Qing and Su, Weiqiang and Liu, Haibin and Dong, Xiaomao and Wu, Mengwu},
journal = {International Journal of Metalcasting},
year = {2026},
doi = {10.1007/s40962-026-02058-3},
url = {https://doi.org/10.1007/s40962-026-02058-3}
}