Fractal Analysis of the Pore Structure of Composite Sorbents Based on Lignite Coke
Аннотация
Abstract The pore structure of composite sorbents based on lignite coke is analyzed by means of fractal theory. The fractal sample dimensions are calculated using the Frenkel–Halsey–Hill (FHH) model, for isotherms of low-temperature nitrogen adsorption at 77 K obtained using an ASAP-2020 system. According to the model, the dependence of ln V on ln [ln ( P 0 / P )] should be a straight line of negative slope S , from which the fractal dimension D may be calculated. However, the correct D value will only be obtained if the appropriate section of the line is selected. In the present work, the first linear section in the range between a monolayer coating and a multilayer coating is selected, in the portion where no surface smoothing is seen. The minimum coating thickness n in the selected range of relative pressure is 1.0. The maximum n is close to 1.3 for all the samples. Analysis of the results shows that the fractal dimensions of the composite sorbents based on lignite coke are between 2.31 and 2.52. In the oxidation of lignite by nitric acid and modification by iron salts, the textural characteristics grow on account of the formation of new pores and decrease in fractal dimension as a result of smoothing of the existing pore surface. Altogether, these factors lead to the formation of a pore system that is more orderly in shape and size.